Produces smooth depositsĀ copper plating for both vat and barrel. High rate of deposition is possible due to increased cathode efficiency. Easily maintained bath. Fine grained, non-porous 5-50 micron of copper deposited. Better anode corrosion and extremely useful for strike coating on Zinc based die-castings.
Cyno Rochelle Copper Salt 2160 | 150-250 gms/ltr |
---|---|
Temperature | 45-50 oC |